PRODUCTS

  • Mattress & Topper System

    Visco-Elastic Foam System consists of Polyol system and ISO system. Polyol system is classified into 2 series, Slab Foam 'SBS-8050N' and Mold Foam 'SMS-7045N'.
    ISO system is only 1 grade, 'SIS-845'
    Memory foam system is the customer-oriented product and essential physical properties should be checked ahead.

    1. Density       2. Hardness     3. Recovery Time    
    4. Temperature Sensitivity     5. Cell Openness     6. Surface Softness
    7. Surface Stickiness     8. Tear Strength

    Mattress & Topper System

    Visco-Elastic Foam System consists of Polyol system and ISO system. Polyol system is classified into 2 series, Slab Foam 'SBS-8050N' and Mold Foam 'SMS-7045N'.
    ISO system is only 1 grade, 'SIS-845'
    Memory foam system is the customer-oriented product and essential physical properties should be checked ahead.

    1. Density       2. Hardness     3. Recovery Time    
    4. Temperature Sensitivity     5. Cell Openness    
    6. Surface Softness 7. Surface Stickiness    
    8. Tear Strength

  • Batch & Slab Foam

    Application : Mattress, Topper, Sofa, Cushion

    Density Porosity
    L/min
    Hardness
    ILD 25%
    Recovery
    Time
    Mixing
    Ratio
    A. General Foam
    1. SBS-8050N 80 ~ 50 ± 3.0 0 ~ 5.0 13.0 ~ 6.0 ± 1.0 1.0 ~ 5.0 100 : 45~47
    B. Air Permeable Foam
    1. SBS-6050A 50 ± 3.0 10 ~ 50 6.0 ± 1.0 5.0 ~ 10 100 : 45 ~ 47
    C. ISO System
    SIS-845 Modified MDI system
  • Batch & Slab Foam

    Application : Mattress, Topper, Sofa, Cushion

    Density Porosity
    L/min
    A. General Foam
    1. SBS-8050N 80 ~ 50 ± 3.0 0 ~ 5.0
    B. Air Permeable Foam
    1. SBS-6050A 50 ± 3.0 10 ~ 50
    C. ISO System
    SIS-845 Modified MDI system
    Hardness
    ILD 25%
    Recovery
    Time
    Mixing
    Ratio
    A. General Foam
    13.0 ~ 6.0 ± 1.0 1.0 ~ 5.0 100 : 45~47
    B. Air Permeable Foam
    6.0 ± 1.0 5.0 ~ 10 100 : 45 ~ 47
    C. ISO System
    Modified MDI system

Using Method

1. Polyol and Modified MDI system should be stored at 24 ± 2.0℃.
2. Polyol system should be vigorously pre-mixed at least 10 mins in a working tank for fine cell.
3. Polyol system should be mixed about 30 seconds in a foaming head.
4. After that, MDI modified system is put and should be mixed about 10 seconds.
5. In addition, for TDI system, adding SUT-9 into polyol system is necessary.